Testing acc. to ISO 3377-1: Leather - Physical and mechanical tests - Determination of tear load - Part 1: Single edge tear
Material
Industry
Publisher
Testing methods
Our test laboratory performs testing in accordance with DIN EN ISO 3377-1 using an accredited procedure. The standard specifies a method for determining the tear load of leather using the single edge tear method. It measures the force required to propagate an existing cut under defined tensile loading conditions.
Tear resistance is an important mechanical quality characteristic of leather. It describes the resistance to the propagation of an existing tear and therefore differs from tensile strength, which evaluates the load-bearing capacity of an undamaged specimen. The test method enables a standardised comparison of the tear propagation behaviour of different types of leather.
Applications
The test method is applicable to all types of leather. These include chrome-tanned, vegetable-tanned and other types of tanned leather, as well as leather with different thicknesses, mechanical properties and surface finishes.
Tear resistance testing is particularly relevant for automotive leather, upholstery and furniture leather, footwear leather, clothing leather, leather goods and technical leather products. It is used to assess mechanical durability and supports material development, quality assurance and product testing.
Tear resistance is especially important for leather components containing cut edges, seams, perforations or other structural weaknesses from which tears may initiate and propagate under mechanical loading.
Test Procedure According to ISO 3377-1
Rectangular leather specimens with a defined cut along one short edge are prepared. The standard specimens measure 70 × 40 mm. The specimens are conditioned according to DIN EN ISO 2419 and taken in two material directions, parallel and perpendicular to the backbone of the leather. Leather thickness is determined in accordance with DIN EN ISO 2589.
The two legs formed by the cut are clamped into the grips of a tensile testing machine and pulled apart at a constant test speed of (100 ± 20) mm/min. This causes the existing tear to propagate in a controlled manner. The forces occurring during tear propagation are continuously recorded as a force-extension curve.
The tear load is determined from the force values recorded during tear propagation. For evaluation, the sequence of force peaks is divided into four sections. The result is calculated from the two middle sections, preferably using electronic evaluation. The mean tear load is expressed in newtons (N).
Testing is performed in both material directions, allowing the directional dependence of tear resistance to be assessed. The mean tear loads for the two directions are reported separately. If required, an additional overall mean value can be calculated.
Related Tests
DIN EN ISO 3377-2 – Determination of Tear Load of Leather Using the Double Edge Tear Method describes an alternative method for determining tear load. Unlike the single edge tear method, this procedure uses a specimen with two opposing cuts. DIN EN ISO 3376 – Determination of Tensile Strength and Percentage Elongation of Leather is used to evaluate tensile strength and elongation behaviour under uniaxial tensile loading. For determining material thickness, FILK offers DIN EN ISO 2589 – Determination of Thickness of Leather. Leather thickness is an important parameter for describing materials and comparing mechanical test results. DIN EN ISO 23910 – Measurement of Stitch Tear Resistance of Leather evaluates the resistance of leather to tearing at a defined stitch point.
Further methods for determining resistance to tear propagation can be found in our specialist category Tear Tests and the corresponding subcategory Single Edge Tear.
A comprehensive overview of additional mechanical and physical test methods is available in our Overview of Physical Testing. Further standards, specifications and testing services can be explored using the search function in our Accredited Test Laboratory Service Overview.