DIN EN 1876-2 Loop Impact Test (accredited)

Testing acc. to EN 1876-2: Rubber or plastics coated fabrics - Low temperatures tests - Part 2: Impact test on loop

Our test laboratory performs testing according to DIN EN 1876-2 using an accredited test method to determine the behaviour of rubber- or plastics-coated textiles at low temperatures. The loop impact test examines whether a coated material withstands sudden deformation after defined exposure to cold or develops incipient cracks and cracks in the coating. The method is suitable only for materials that can be formed at room temperature into the loop required for testing without damage.

Test procedure

For the test, representative specimens are taken from the coated textile in both the longitudinal and transverse directions, conditioned and formed into a loop. The specimens are then stored in a low-temperature chamber at the specified test temperature. While still cold, a falling hammer strikes the material loop, producing rapid bending and deformation.

After testing, the specimens are examined under low magnification for incipient cracks and cracks in the coating. By carrying out tests at progressively lower temperatures, the brittleness limit temperature can be determined. The temperature at which the specified failure criteria are reached is then assessed.

Applications of the test

Testing according to DIN EN 1876-2 is used to assess the low-temperature resistance and tendency to embrittlement of coated textiles. Polymer coatings may become increasingly hard and brittle as the temperature decreases. The sudden impact loading of a cooled material loop makes such changes clearly visible. The method is therefore suitable for the comparative evaluation of different coatings, formulations and material constructions with regard to their behaviour at low temperatures.

Typical test materials and applications include:

  • artificial leather and other plastics-coated textiles,

  • rubber-coated textile fabrics,

  • coated seat and covering materials for vehicle interiors,

  • coated trim and upholstery materials for automotive applications,

  • furniture and upholstery covering materials with polymer coatings,

  • flexible coated materials for interior and contract furnishing,

  • technical coated textiles and coated textile composite materials.

The test is particularly important for materials that are exposed to low temperatures during transport, storage or use and must withstand mechanical loads under these conditions. It is therefore suitable for material development and quality assurance as well as for comparative material testing and the investigation of cold-related damage.

Related standards

As a directly related test, FILK also offers DIN EN 1876-1, which evaluates the behaviour of coated textiles at low temperatures by means of a bending test. However, the results of the two methods are not directly comparable. DIN EN ISO 22751 can also be used to determine the bending properties of rubber- or plastics-coated textiles. DIN EN ISO 32100 evaluates the flex resistance of such materials using the flexometer method and thus enables assessment of their behaviour under repeated flexing.



Inquiry to Test Laboratory