ISO 11357-6: Plastics - Differential scanning calorimetry (DSC) - Part 6: Determination of oxidation induction time (isothermal OIT) and oxidation induction temperature (dynamic OIT)
Material
Industry
Publisher
Testing categories
Our test laboratory performs testing according to DIN EN ISO 11357-6 to determine the oxidation induction time and oxidation induction temperature of plastics using an accredited test method. Differential scanning calorimetry (DSC) is used to determine how long, or up to which temperature, a polymeric material resists oxidative degradation.
The test is particularly suitable for stabilized polyolefins such as polyethylene (PE) and polypropylene (PP). It provides a comparative measure of the effectiveness of the stabilizer system but does not directly determine the concentration of individual antioxidants.
Applications
OIT testing is used for quality control of plastic raw materials, compounds and finished products. Typical applications include films, plastic sheeting, pipes, moulded parts, polymeric coatings and technical plastic components.
The results allow different formulations, production batches and processing conditions to be compared in terms of their oxidation stability. Testing can also provide indications of changes in stabilization following processing or ageing exposure.
Testing according to DIN EN ISO 11357-6
During DSC analysis, a defined plastic specimen is exposed to an oxygen or air atmosphere under controlled temperature conditions. The onset of the exothermic oxidation reaction is identified from the change in heat flow.
The standard distinguishes between two methods:
Isothermal OIT: The specimen is first heated to a specified test temperature under nitrogen. After switching to oxygen or air, the time until the onset of oxidation is determined. The result is reported in minutes.
Dynamic OIT: The specimen is heated at a specified rate under oxygen or air. The temperature at which oxidation begins is determined and reported in °C.
The results depend on factors including the test temperature or heating rate, gas atmosphere and specimen preparation. Meaningful material comparisons therefore require comparable test conditions.
Related tests
For additional thermal characterization, FILK offers DIN EN ISO 11357-2 – Determination of glass transition temperature and glass transition step height and DIN EN ISO 11357-3 – Determination of temperature and enthalpy of melting and crystallization .
Thermogravimetric analysis according to DIN EN ISO 11358-1 can also be used to determine changes in the mass of a plastic as a function of temperature or time. This method complements DSC when evaluating thermal decomposition behaviour.