FILK-QMA-1088 Collagen: Tensile Strength (accredited)

Testing acc. to FILK standard: Collagen fleece - Determination of tensile strength and percentage elongation

Our test laboratory performs testing in accordance with FILK-QMA-1088 using an accredited procedure. This in-house test method is used to determine the tensile strength and percentage elongation of collagen fleece. It provides information about the mechanical strength and deformation behaviour of collagen-based nonwoven materials.

The test supports material development, quality assurance and comparative characterisation of collagen fleece, particularly for technical and medical applications.

Related Tests

FILK-QMA-1095 – Determination of Tensile Strength and Percentage Elongation of Pericardium provides a corresponding method for the mechanical characterisation of another biogenic material.  FILK-QMA-1001 – Determination of Thickness of Leather, Collagen Fleece and Pericardium offers a complementary method for measuring material thickness.

Further methods for evaluating mechanical material properties can be found in our specialist category Tensile Tests and in our Overview of Physical Testing.

A comprehensive overview of our testing services, including a search function for additional standards, specifications and test methods, is available in our Accredited Test Laboratory Service Overview.



Inquiry to Test Laboratory

Contact

FILK Freiberg Institute gGmbH
Meißner Ring 1-5
09599 Freiberg

GERMANY

Fon: +49-(0)3731-366-0
Fax: +49-(0)3731-366-130
E-Mail: mailbox@filkfreiberg.de