VDA 230-217 Low Temperature Resistance (accredited)

Testing acc. to VDA 230-217: Plastic Roll Goods for Motor Vehicel Interior Trim Test of Low Temperature Resistance

Our test laboratory performs testing according to VDA 230-217 as an accredited test method to determine the low-temperature resistance of plastic roll goods used for motor vehicle interior trim. The test evaluates the behaviour of materials under impact or rapid bending at low temperatures. VDA 230-217 specifies two test methods: Method A – impact test on loop and Method B – ball impact test.

The test is particularly relevant to flexible surface and roll materials used in vehicle interiors. These include plastic roll goods, materials based on plasticised PVC and coated textile materials. Especially in plasticised PVC materials, mechanical behaviour can change considerably at low temperatures.

Testing according to VDA 230-217

In Method A – impact test on loop, the specimen is formed into a loop and subjected to an impact from a freely falling weight at the specified test temperature. Specimens are tested in both the machine and cross-machine directions. Drop height and drop-weight mass may be specified by the customer or the applicable material specification.

In Method B – ball impact test, the specimen is positioned on a rigid support with the surface to be tested facing upwards. After conditioning at the specified low temperature, a steel ball is dropped from a defined height onto the surface. In addition to roll materials, this method can also be applied to specimens taken from suitably flat areas of moulded components.

If no other test temperature is specified by the customer or an applicable specification, VDA 230-217 specifies testing at −30 °C. After the low-temperature impact, the specimens are returned to room temperature and visually examined for changes and damage.

Applications of the test

VDA 230-217 is used to assess whether flexible vehicle interior materials retain sufficient resistance to sudden mechanical loading at low temperatures. The evaluation can identify cracks, fractures, stress whitening and other material changes resulting from low-temperature exposure and impact.

The two methods represent different loading conditions. The impact test on loop combines pronounced bending of the material with sudden impact loading, whereas the ball impact test applies a localized impact to the material surface. Selection of the appropriate method depends on the intended use of the material in the vehicle or on the relevant material specification.

Related tests

Closely related standardized methods include low-temperature testing of coated fabrics according to DIN EN ISO 4675 and the low-temperature tests specified in EN 1876-1 and EN 1876-2. For evaluating additional mechanical properties of vehicle interior surface materials, FILK also performs the accredited scratch and scuff test according to VDA 230-218.

Further information can be found in our overview of VDA tests and specifications and in the test laboratory overview with a search function for standards, specifications and testing services. 



Inquiry to Test Laboratory

Contact

FILK Freiberg Institute gGmbH
Meißner Ring 1-5
09599 Freiberg

GERMANY

Fon: +49-(0)3731-366-0
Fax: +49-(0)3731-366-130
E-Mail: mailbox@filkfreiberg.de